The Evaluation of the Comparative Corrosion Behaviour of Conventional and Low-Nickel Austenitic Stainless Steel: Hercules™ Alloy
Austenitic stainless steels require approximately 8% Ni to maintain austenitic microstructure at room temperature for alloys such as 304 stainless steel (304SS). Ni contributes approximately 60% of the total material cost and its price fluctuates, making the cost of austenitic stainless steel unpred...